Temper embrittlement can not be prevented if the material contains _____________ and is exposed in the______________.
critical levels of the embrittling impurity elements
embrittling temperature range
To minimize the possibility of brittle fracture during startup and shutdown, many refiners use a _____________ to limit system pressure to about _________ of the maximum design pressure for temperatures below a Minimum Pressurization Temperature (MPT). Note that MPT
is not a single point but rather a __________ which defines safe operating conditions to minimize the likelihood of brittle fracture.
pressurization sequence
25 percent
pressure-temperature envelope
MPT’s generally range from ________for the earliest, most highly temper embrittled steels, down to _________ for newer, temper embrittlement resistant steels (as required to also minimize effects of hydrogen embrittlement).
350°F (171°C)
125°F (52°C) or lower
If weld repairs are required, the effects of temper embrittlement can be temporarily reversed (de-embrittled) by ______________, and __________. It is important to note that re-embrittlement will occur over time if the material is re-exposed to the __________.
heating at 1150°F (620°C) for two hours per inch of thickness
rapidly cooling to room temperature
embrittling temperature range
Author
egf4201
ID
349538