API 571 CUI

  1. CUI is an inspection concern for insulated carbon steel equipment that operates between:
    10-350°F
  2. CONFLICT - CUI is an inspection concern for insulated austenitic stainless steel equipment that operates between:
    140-400°F

    Per API 510; Austenitic is 140-350°F and Duplex is 280-350°F.
  3. CUI is an inspection concern for insulated vessels that operate at 500°F and are:
    in intermittent service
  4. CUI is most severe when metal temperatures are between:
    212-350°F
  5. If the metal temperature increases, while still in the CUI temperature range, the corrosion rate will:
    Increase
  6. CUI on carbon steel or low alloy materials appears as:
    Localized pitted or localized wall loss
  7. CUI on 300 Series SS materials appears as:
    Cracking, localized pitting, or localized wall loss.
  8. What causes CUI cracking on 300 series SS  materials?
    Chlorides
  9. Which of the following is NOT a method to inspect for CUI?




    B) MFL
Author
Gibby
ID
333977
Card Set
API 571 CUI
Description
API 571 CUI
Updated