CUI is an inspection concern for insulated carbon steel equipment that operates between:
10-350°F
CONFLICT - CUI is an inspection concern for insulated austenitic stainless steel equipment that operates between:
140-400°F
Per API 510; Austenitic is 140-350°F and Duplex is 280-350°F.
CUI is an inspection concern for insulated vessels that operate at 500°F and are:
in intermittent service
CUI is most severe when metal temperatures are between:
212-350°F
If the metal temperature increases, while still in the CUI temperature range, the corrosion rate will:
Increase
CUI on carbon steel or low alloy materials appears as:
Localized pitted or localized wall loss
CUI on 300 Series SS materials appears as:
Cracking, localized pitting, or localized wall loss.
What causes CUI cracking on 300 series SS materials?
Chlorides
Which of the following is NOT a method to inspect for CUI?
A) De-insulate and visually inspect
B) MFL
C) Guided Wave UT
D) Real-time Profile RT
E) Neutron Backscatter
B) MFL